ALLOY |
DESCRIPTION |
CLASSIFICATION |
PHYSICALS |
| F15 FC |
A very tough alloy for use in repair of columns and cylinders
and other areas subject to cracking. |
Fe-Ni-Cr-Mo
6% alloy |
15-20 Rc as welded
115,000 psi tensile |
| F25 FC |
This alloy is used to buildup worn areas subject to high
impact and compressive loads such as rams, sow blocks and shanks. |
Fe-Ni-Cr-Mo
8% alloy |
25-30 Rc as welded
132,000 psi tensile |
| F35 FC |
For reclamation of hammer die impressions. This alloy is
similar in wear properties to die block with a number 2 temper. |
Fe-Ni-Cr-Mo
10% alloy |
32-37 Rc as welded 165,000 psi tensile |
| F40 FC |
For hammer die impressions when more abrasion resistance is
needed than F35 FC provides. |
Fe-Ni-Cr-Mo
12% alloy |
38-43 Rc as welded 182,000 psi tensile |
| F45 FC |
For shallow hammer and press die applications |
Fe-Ni-Cr-Mo
14% alloy |
42-47 Rc as welded 186,000 psi tensile |
| F54 FC |
Provides machinable deposit for press die applications |
5% Cr Hot Work |
38-42 Rc as welded |
| F58 FC |
A 5% Cr Hot Work alloy for press dies. |
AISI H-12 |
51-56 Rc as welded |
| F580 FC |
A higher alloy version of F58 that withstands higher service
temperatures without softening |
AISI H-12 type with higher W and Mo |
51-56 Rc as welded |
| F63 FC |
For shallow hammer dies with high duty cycles and press dies
subjected to high heat and stresses when a machinable deposit is required. |
9% Cr Hot Work |
42-46 Rc as welded |
| F64 FC |
For use on press dies subjected to high heat and stresses. |
11% Cr Hot Work |
48-53 Rc as welded |
| F65 FC |
For shallow hammer dies and high cycles and press dies
subjected to high heat and stresses. |
9.5% Cr Hot Work |
49-52 Rc as welded |
| 6 FC |
Cobalt #6alloy that maintains hardness at high
temperatures |
AWS ECoCr-A |
42-46 Rc as welded |
| 21 FC |
Cobalt #21 alloy that maintains hardness and impact
properties at high temperatures. |
Co-Cr-Mo |
28-33 Rc as welded |
| 2101 FC |
Offers superior resistance to heat checking, spalling,
chipping and erosion over our 21 alloy. |
Co-Cr-Mo-Cb |
33-38 Rc as welded 45+ Rc work hardened |
| F110 FC |
Used for overlaying of forging dies and components
subject to high temperatures and impacts. |
AWS ENiCrMo-5 |
100,000 psi tensile min. 20 Rc as welded |
| F111 FC |
An excellent underlayment for harder nickel base
alloys on high temperature forging dies. |
modification of AWS ENiCrMo-5 |
20 Rc as welded
40 Rc work hardened |
| F112 FC |
For forging surfaces exposed to high temperatures and
long contact times. |
modification of AWS ENiCrMo-3 |
110,000 psi tensile
30% Elongation min |
| F114 FC |
For overlay of rotary forging dies subjected to high
temperatures and stresses. |
modified
UDIMET®520 |
25-30 Rc as welded |
| F115 FC |
For overlay of rotary forging dies subjected to high
temperatures and stresses |
modified
UDIMET®520 |
30-35 Rc as welded |
| F116 FC |
For overlay of rotary forging dies subjected to high
temperatures and stresses |
modified
UDIMET®520 |
35-40 Rc as welded |